首页> 外国专利> The high surrender difference in elevation strength hot rolling steel sheet and the high surrender difference in elevation strength melting galvanized steel sheet, and the high surrender difference in elevation strength alloy melting galvanized steel sheet and the production mannered null mass which are superior in weldability

The high surrender difference in elevation strength hot rolling steel sheet and the high surrender difference in elevation strength melting galvanized steel sheet, and the high surrender difference in elevation strength alloy melting galvanized steel sheet and the production mannered null mass which are superior in weldability

机译:高强度热轧钢板的屈服差高,高强度熔融镀锌钢板的屈服差高,高强度合金熔融镀锌钢板的高屈服差和焊接性优良的生产方式零质量

摘要

PROBLEM TO BE SOLVED: To provide a high yield ratio and high strength hot rolled steel plate and a high yield ratio and high strength galvanized steel plate, both having excellent weldability and ductility, and to provide a high yield ratio and high strength alloyed galvanized steel plate and its manufacturing method.;SOLUTION: The high yield ratio and high strength hot rolled steel plate having excellent weldability and ductility is a steel containing, by mass%, over 0.030 to less than 0.10 of C, 0.35 to 0.80 of Si, 1.7 to 3.2 of Mn, 0.001 to 0.02 of P, 0.0001 to 0.006 of S, ≤0.060 of Al, 0.0001 to 0.0070 of N, 0.01 to 0.055 of Ti, 0.012 to 0.055 of Nb, 0.07 to 0.55 of Mo, 0.0005 to 0.0040 of B and the balance of iron and inevitable impurities, and the steel has the yield ratio of 0.68 or more and less than 0.92, ≥1.0 X-ray intensity ratio on a {110} plane in a layer at a depth corresponding to 1/8 thickness of the steel plate and parallel to the plate face, and ≥780 MPa highest tensile strength (TS).;COPYRIGHT: (C)2005,JPO&NCIPI
机译:要解决的问题:提供高焊接效率和延展性的高屈服比和高强度热轧钢板以及高屈服比和高强度镀锌钢板,并提供高屈服比和高强度合金化镀锌钢板解决方案:具有优良的可焊性和延展性的高屈服比和高强度热轧钢板是按质量%计,C含量超过0.030至小于0.10,Si含量为0.35至0.80,1.7 Mn的3.2至0.2,P的0.001至0.02,S的0.0001至0.006,Al的0.060,N的0.0001至0.0070,Ti的0.01至0.055,Nb的0.012至0.055,Mo的0.07至0.55,0.0005至0.0040的钢的屈服比为0.68以上且小于0.92,在{110}面的层中的深度对应于1时,钢的屈服比为0.68以上且小于0.92,≥1.0X射线强度比。钢板的/ 8厚度并平行于钢板表面,且高780 MPa EST拉伸强度(TS)。;版权所有:(C)2005,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号