PROBLEM TO BE SOLVED: To provide a curtain coating method carried out by falling down a curtain 10 comprising a plurality of layers of liquid films and applying a plurality of layers of films on the surface of a travelling board 11 wherein the liquid film layer comprises a broad layer 12 and narrow layer 13 and a film thinning phenomenon that the thickness of a part of the film is made thin to form a thinned film part 14 does not occur.;SOLUTION: In the curtain coating method, the narrow layer 13 comprises a solution of a high molecular material having a molecular weight of 3,000-30,000, the broad layer 12 comprises a solution of a high molecular material having the molecular wight of 10,000-30,000, a factor Z is determined by following formula (4a) and the relationship between the molecular weight of the broad layer 12 and Z satisfies following formula (1b) and the relationship between the molecular weight of the narrow layer and Z satisfies following formula (2b), that are (1b); Z≤Y1=A1×broad film molecular weight+B1 (2b); Z≤Y2=A2×narrow film molecular weight+B2 and(4a); Z=Z1=-10×(broad film surface tension - narrow film surface tension)+9.;COPYRIGHT: (C)2006,JPO&NCIPI
机译:解决的问题:提供一种幕帘涂覆方法,该方法通过使包括多层液膜的幕帘10掉落并在移动板11的表面上涂覆多层膜而进行,其中液膜层包括一层宽层12和窄层13以及膜变薄的现象不会发生,即膜的一部分的厚度变薄以形成薄的膜部分14。解决方案:在幕涂法中,窄层13包括分子量为3,000-30,000的高分子材料的溶液,宽层12包括分子量为10,000-30,000的高分子材料的溶液,因数Z由下式(4a)确定,并且宽层12和Z的分子量满足下式(1b),且窄层和Z的分子量满足下式(2b),即(1b); Z≤ Y1 = A1×宽膜分子量+ B1(2b); Z≤ Y2 = A2×窄膜分子量+ B2和(4a); Z = Z1 = -10×(宽膜表面张力-窄膜表面张力)+9 .;版权:(C)2006,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号