PROBLEM TO BE SOLVED: To provide a curing-type water-based film protecting composition environmentally-friendly and excellent in film protecting properties and easily removable properties, to provide a curing-type water-based film protecting agent obtained by using the composition, and to provide a water-based film protecting coat.;SOLUTION: This curing-type water-based film protecting composition comprises a hydrophilic polyrotaxane, wherein the hydrophilic polyrotaxane includes a cyclic molecule, a straight-chain molecule, and sealing groups and the straight-chain molecule or the cyclic molecule has a hydrophilic modifying group. An inclusion amount of the cyclic molecule is 0.06 to 0.61. A molecular weight of the straight-chain molecule is 1,000 to 60,000. The curing-type water-based film protecting agent comprises the curing-type water-based film protecting composition, wherein the composition is contained in an amount of 50-90%. The water-based film protecting coat is formed by solidifying the curing-type water-based film protecting agent, wherein a thickness of the protecting coating is 100-1,000 μm.;COPYRIGHT: (C)2007,JPO&INPIT
机译:要解决的问题:提供一种对环境友好且具有优异的膜保护性能和易除去性能的固化型水基膜保护组合物,提供一种通过使用该组合物获得的固化型水基膜保护剂,以及解决方案:该固化型水基膜保护组合物包含亲水性聚轮烷,其中亲水性聚轮烷包括环状分子,直链分子和密封基团,并且直链-链分子或环状分子具有亲水性修饰基团。环状分子的包含量为0.06〜0.61。直链分子的分子量为1,000至60,000。固化型水基膜保护剂包含固化型水基膜保护组合物,其中该组合物的含量为50-90%。通过固化固化型水基膜保护剂来形成水基膜保护涂层,其中保护膜的厚度为100-1,000μm。版权所有:(C)2007,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号