A method for producing a fire brick for a bottom portion of a float bath by the use of a clayey material containing 30 to 45 mass % of AlO, 50 to 65 mass % of SiO, and having a content of NaO of 1 mass % or less, characterized in that a potassium compound is added in such a manner that the resultant fire brick for a float bath has a KO content of 2 to 4 mass %. A fire brick for use in a bottom portion of a float bath of a flat glass produced by the float method, which is produced by the above method, can inhibit the reaction with the NaO in glass on the surface thereof and thus can prevent a flaking phenomenon.
机译:一种通过使用包含30至45质量%的AlO,50至65质量%的SiO,且NaO的含量为1质量%的粘土材料制造浮法浴的底部的耐火砖的方法。更小的特征在于,以使得到的用于浮法的耐火砖的KO含量为2-4质量%的方式添加钾化合物。通过上述方法制造的,用于通过浮法制造的平板玻璃的浮法浴的底部中使用的耐火砖可以抑制与玻璃中的NaO在其表面上的反应,因此可以防止剥落。现象。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号