首页> 外国专利> A METHOD FOR FABRICATING AN OPEN-POROUS METAL FOAM BODY, A METAL FOAM BODY FABRICATED THIS WAY AS WELL AS ITS APPLICATIONS

A METHOD FOR FABRICATING AN OPEN-POROUS METAL FOAM BODY, A METAL FOAM BODY FABRICATED THIS WAY AS WELL AS ITS APPLICATIONS

机译:一种制造多孔金属泡沫体的方法,一种以此方法制造的金属泡沫体及其应用

摘要

The invention relates to a method for fabricating an open-porous metal foambody with a nickel base alloy, to a metal foam body fabricated this way aswell as advantageous applications for the separation of specific componentsand pollutants from fluid flows. On the occasion, according to the set objectopen-porous metal foam bodies which have improved mechanical properties, andin addition an enlarged specific surface and/or increased surface roughnessare to be provided. During fabricating it is proceeded such that an open-porous base foam body made of nickel or a nickel base alloy is coated with aliquid binding agent. Subsequent to this, a mixture of a powdery nickel basealloy and an organic component the temperature of phase transformation ofwhich is at least 30 degrees centigrade from its solid phase to the liquidphase is deposited. The temperature should then be below the respectivetemperature of phase transformation. By means of thermal treatment the bindingagent and the organic component are expelled, a portion of the powderparticles is sintered, and a further portion of the powder particles isconnected with the surface of the base foam body in a material-fit manner viasintering bridges.
机译:本发明涉及一种开孔金属泡沫的制造方法镍基合金制成的主体,然后以这种方式制造的泡沫金属制成以及分离特定成分的有利应用以及来自流体流动的污染物。场合,根据设定对象具有改善的机械性能的开孔金属泡沫体,以及另外,比表面积增大和/或表面粗糙度增大将被提供。在制造过程中,要进行以下操作:由镍或镍基合金制成的多孔基础泡沫体涂有液体粘合剂。随后是粉状镍基的混合物合金与有机组分相变温度。从固相到液体至少30摄氏度相沉积。然后温度应低于各自的温度相变温度。通过热处理结合排出剂和有机成分,一部分粉末烧结颗粒,然后将另一部分粉末通过材料配合方式与基础泡沫体的表面连接烧结桥。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号