sintered ore for steel with improved recovery method

机译:改进回收率的钢烧结矿

摘要

The present invention relates to a method for producing sintered ore for iron using a di elsik sintering. According to the method the sintered ore produced, the sintering bed on the raw material charge layer a surface layer of approximately 50 to 100mm deep at the front end of the cheunghu for adjusting the cut-off plate in the minutes for sintering coke as a heat source to promote the melt formed in the charging device 16, supply. At this time, the minute coke is transferred from the transport vehicle, are stored in the hopper, the amount dispensed from the hopper, two-way screw feeder 10, the guide plate 12 and the wind is installed to the front end of the cut-off plate 16 dispersed supply to the raw material packed layer in the surface layer by dispersing device 14 is mixed with the blended material. The method can improve the recovery rate and the strength of the sintered ore surface layer by increasing the amount of heat and melt plastic production.; Sintering, the surface layer, melt-minute coke, recovery
机译:用狄尔斯克烧结生产铁烧结矿的方法技术领域本发明涉及一种利用狄尔斯克烧结生产铁烧结矿的方法。根据所生产的烧结矿的方法,在原料装料层上的烧结床在长湖的前端深约50至100mm的表层,以便在几分钟内调节分切板,从而将焦炭作为热量进行烧结。源促进在充电装置16中形成的熔体供给。此时,微小的焦炭从运输车辆中转移出来,并存储在料斗中,从料斗中分配的量,双向螺旋进料器10,导向板12和风安装在切口的前端通过分散装置14向表层中的原料填充层分散供给的脱模板16与混合材料混合。通过增加热量和熔融塑料的生产量,该方法可以提高烧结矿表层的回收率和强度。烧结,表面层,熔融焦炭,回收

著录项

  • 公开/公告号KR100928830B1

    专利类型

  • 公开/公告日2009-11-27

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20020084722

  • 发明设计人 강주;김성완;김재왕;

    申请日2002-12-27

  • 分类号C22B1/16;

  • 国家 KR

  • 入库时间 2022-08-21 18:33:45

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号