首页> 外国专利> Sintered ore manufacturing method for improving recovery rate of sintered ore

Sintered ore manufacturing method for improving recovery rate of sintered ore

机译:提高烧结矿回收率的烧结矿制造方法

摘要

The present invention not only improves the recovery rate of sintered ore when manufacturing sintered ore using low iron oxides such as mill scale and metal waste generated in various metal processing processes such as steelmaking and cutting such as rolling and wire rod as iron ore sintering raw materials. The present invention relates to a method for producing a sintered ore such that the oil, which is often buried in these lower iron oxides, hardly adversely affects the sintering dust collector.;Low iron oxides such as Fe, FeO, Fe 3 O 4 or lower iron oxides such as mill scale, steel sludge, and metal iron that occur in industrial processes such as iron and metal processing, with their respective minerals mixed. When used as a sintering raw material, these low iron oxides are separately mixed with silica, which is usually added as a sintering raw material, and then charged into the upper part of the sintered raw material layer and sintered to improve the strength and the yield of the sintered ore at the upper part of the sintered layer. It is.
机译:本发明不仅提高了使用低氧化铁(例如氧化铁皮)和在诸如炼钢和切割(例如轧制和盘条)的各种金属加工过程中产生的金属废料作为铁矿石烧结原料制造烧结矿时的回收率。 。本发明涉及一种烧结矿的生产方法,使得通常埋在这些低级氧化铁中的油几乎不会对烧结集尘器产生不利影响。低铁氧化物,例如Fe,FeO,Fe 3 O 4 或更低级别的氧化铁,例如轧制氧化皮,钢渣和金属铁,它们在诸如铁和金属加工的工业过程中发生,并且将各自的矿物混合在一起。当用作烧结原料时,这些低铁氧化物分别与二氧化硅混合,通常将其作为烧结原料加入,然后装入烧结原料层的上部并进行烧结以提高强度和成品率在烧结层上部的烧结矿的厚度。它是。

著录项

  • 公开/公告号KR19990010562A

    专利类型

  • 公开/公告日1999-02-18

    原文格式PDF

  • 申请/专利权人 김종진;

    申请/专利号KR19970033368

  • 发明设计人 서인국;박인규;김기수;

    申请日1997-07-18

  • 分类号C22B1/16;

  • 国家 KR

  • 入库时间 2022-08-22 02:17:58