首页> 外国专利> METHOD OF PRODUCTION OF NANO-DISPERSED WEAR RESISTANT COMPOUND (NDWRC) AND LUBRICATING COMPOSITION CONTAINING IT

METHOD OF PRODUCTION OF NANO-DISPERSED WEAR RESISTANT COMPOUND (NDWRC) AND LUBRICATING COMPOSITION CONTAINING IT

机译:纳米分散抗磨化合物(NDWRC)的生产方法及包含它的润滑成分

摘要

FIELD: machine building.;SUBSTANCE: mineral, preliminary crumbled to powder, is introduced into process fluid; produced suspension is treated by ultra-sound at power of emission not less, than 5 kWt and duration not less, than 10 minutes. Further, process fluid is drained, while the residue compound is dispersed in a liquid lubricant material containing a surface active substance forming colloid solution with particles of a mineral. Produced mixture is settled and suspension, formed over sediment, is used as additive to main lubricating material. Natural mineral contains in wt %: serpentine (lizardite and chrisotile) 80-87, chlorite 2-3, magnetite 1-2, amakinite 1-2, calcite 0.5-1, radio-amorphous phase 8.5-12. Water, or alcohol or kerosene are preferably used as process fluid. Lubricant composition contains main lubricating material and compound produced by the above described method.;EFFECT: reduced wear of friction units, reduced losses for friction, increased efficiency of machines and equipment, and reduced consumption of lubricating materials.;5 cl, 1 tbl, 2 dwg
机译:领域:机械制造;物质:矿物,先将其粉碎成粉末,然后引入工艺流体中;生产的悬架将通过超声波处理,且发射功率不少于5 kWt,持续时间不少于10分钟。此外,排出工作流体,同时将残余化合物分散在液体润滑剂材料中,该液体润滑剂材料包含与矿物颗粒形成胶体溶液的表面活性物质。沉降产生的混合物,并在沉积物上形成悬浮液,用作主要润滑材料的添加剂。天然矿物的含量为wt%:蛇纹石(蜥蜴石和锂长石)80-87,绿泥石2-3,磁铁矿1-2,石1-2,方解石0.5-1,放射性非晶相8.5-12。优选将水或酒精或煤油用作工艺流体。润滑剂组合物包含主要润滑材料和通过上述方法生产的化合物;效果:减少了摩擦装置的磨损,减少了​​摩擦损失,增加了机器和设备的效率,并减少了润滑材料的消耗; 5 cl,1 tbl, 2 dwg

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号