PROBLEM TO BE SOLVED: To provide a photosensitive resin composition allowing production of a flexographic printing plate having high impact resilience and high notch/crack resistance.;SOLUTION: The liquid photosensitive resin composition for a flexographic printing plate contains 100 pts.mass of a polyurethane prepolymer (a) with an ethylenically unsaturated group, 10 to 150 pts.mass of an ethylenically unsaturated compound (b), and 0.01 to 10 pts.mass of a photoinitiator (c) and contains 5 to 100 pts.mass of a compound expressed by general formula (1) CH2=CH-CO-O-(C3H6O)n-H, as the ethylenically unsaturated compound (b), relative to 100 pts.mass of the polyurethane prepolymer (a) with the ethylenically unsaturated group. In the general formula (1), n represents an integer in a range of 1 to 20.;COPYRIGHT: (C)2012,JPO&INPIT
展开▼
机译:解决的问题:提供一种光敏树脂组合物,该组合物允许生产具有高冲击回弹性和高抗缺口/抗裂性的柔性版印刷板;解决方案:用于柔性版印刷板的液体光敏树脂组合物包含100点质量的聚氨酯。具有烯键式不饱和基团的预聚物(a),烯键式不饱和化合物(b)的质量为10至150 pt,光引发剂(c)的分子量为0.01至10 pts,并含有5至100 pts的质量的化合物由通式(1)CH 2 Sub> = CH-CO-O-(C 3 Sub> H 6 Sub> O) n Sub > -H,作为烯键式不饱和化合物(b),相对于具有烯键式不饱和基团的聚氨酯预聚物(a)的100pts。质量。在通式(1)中,n表示1至20范围内的整数; COPYRIGHT:(C)2012,JPO&INPIT
展开▼