2/kg and a residual magnetization value of 0-10 A m2/kg (however, saturation magnetization valueresidual magnetization value).;COPYRIGHT: (C)2011,JPO&INPIT"/> METHOD FOR MANUFACTURING MAGNETIC BALL FOR BIOTECHNOLOGY, AND MAGNETIC BALL AND MAGNETIC PRODUCT
首页> 外国专利> METHOD FOR MANUFACTURING MAGNETIC BALL FOR BIOTECHNOLOGY, AND MAGNETIC BALL AND MAGNETIC PRODUCT

METHOD FOR MANUFACTURING MAGNETIC BALL FOR BIOTECHNOLOGY, AND MAGNETIC BALL AND MAGNETIC PRODUCT

机译:用于生物技术的磁球的制造方法以及磁球和磁性产品

摘要

PROBLEM TO BE SOLVED: To provide a method for reducing and solving a limitation and a problem accompanied by "a fine particle" and "a micro-plate sample tube".;SOLUTION: The method for manufacturing a magnetic ball used in a biotechnology life science field includes the steps (i) mixing at least two magnetic particles and a resin raw material to prepare a particle dispersion resin raw material, (ii) providing the particle dispersion resin raw material to mold and obtaining a particle dispersion molded article, (iii) grinding and/or polishing the particle dispersion molded article to a spherical shape and forming a magnetic ball with a particle size 0.1 mm or more and 30 mm or less which has a saturation magnetization value of 2-200 A m2/kg and a residual magnetization value of 0-10 A m2/kg (however, saturation magnetization valueresidual magnetization value).;COPYRIGHT: (C)2011,JPO&INPIT
机译:要解决的问题:提供一种减少和解决“细小颗粒”和“微板样品管”所伴随的局限性和问题的方法。科学领域包括以下步骤:(i)将至少两种磁性颗粒和树脂原料混合以制备颗粒分散树脂原料,(ii)将颗粒分散树脂原料提供给模具并获得颗粒分散成型品,(iii )将颗粒分散体成型体研磨和/或抛光成球形,并形成粒径为0.1mm以上且30mm以下的磁球,其饱和磁化值为2-200 A m / kg,剩余磁化值为0-10 A m 2 / kg(但是,饱和磁化值>残余磁化值)。;版权:(C)2011,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号