PPROBLEM TO BE SOLVED: To improve the ununiformity in the wettability of the surface in a silicon carbide fiber-reinforced ceramic matrix composite (CMC), at the time when a steam corrosion resistance coating (EBC) is applied to the surface of the CMC via crystallized glass (BMAS), and to realize the coating with a uniform thickness. PSOLUTION: In the coating, on the surface layer of an SiC-based fiber-reinforced ceramic (CMC) base material 1, an intermediate layer composed of a layer 4 impregnated with a mixture of the crystallized glass (BMAS) composed of BaO-MgO-AlSB2/SBOSB3/SB-SiOSB2/SBand a rare earth silicate, and a CVD-SiC layer 2 obtained by impregnating an SiC layer with a mixture of BMAS and a rare earth silicate, deposited so as to be the porous one on the surface of the base material by a CVD process is formed, and a rare earth silicate layer 5 is further formed on the CVD-SiC layer 2 as a top coat. PCOPYRIGHT: (C)2006,JPO&NCIPI
机译:

要解决的问题:为了改善碳化硅纤维增强陶瓷基复合材料(CMC)中表面的润湿性的不均匀性,在将耐蒸汽腐蚀涂层(EBC)应用于表面时通过结晶玻璃(BMAS)进行CMC,以实现厚度均匀的涂层。

解决方案:在涂层中,在SiC基纤维增强陶瓷(CMC)基体材料1的表面层上,形成一个中间层,该中间层由层4组成,层4浸渍了由以下成分组成的结晶玻璃(BMAS)的混合物: BaO-MgO-Al 2 O 3 -SiO 2 和稀土硅酸盐,以及通过浸渍SiC获得的CVD-SiC层2形成由BMAS和稀土硅酸盐的混合物构成的层,通过CVD法在基材的表面上形成为多孔质,然后在CVD-SiC层上形成稀土硅酸盐层5。 2作为面漆。

版权:(C)2006,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号