The junction mannered null precast reinforced concrete cylinder component of the precast reinforced concrete cylinder component

机译:预制钢筋混凝土圆柱构件的结点为零的预制钢筋混凝土圆柱构件

摘要

PROBLEM TO BE SOLVED: To complete joining work quickly using a hardening filler having good characteristics in a joining method between a PCa column member and a PCa column/beam joint part block in which the hardening filler is injected into a joint space formed between an upper face of a column head of the PCa column member and a lower face of the PCa column/beam joint part block, and into a plurality of insertion holes for column main reinforcements of the PCa column/beam joint part block by injecting the hardening filler into the joint space.;SOLUTION: Cement mortar having fluidity is fed into the joint space 26 to allow it to flow from a lower end of each of the insertion holes 16 for the column main reinforcements so that it may fill the inside of the holes. Before the highest top end of the top ends of the hardening filler rising in the insertion holes reaches an upper end of the corresponding insertion hole, injection of the hardening filler is stopped to leave an unfilled part near the upper end of the insertion hole as a margin. The unfilled part is filled with the hardening filler injected from an upper end of each of the insertion hole.;COPYRIGHT: (C)2006,JPO&NCIPI
机译:解决的问题:为了在PCa柱构件与PCa柱/梁连接部件块之间的连接方法中使用具有良好特性的硬化填料快速完成连接工作,在该方法中,将硬化填料注入到上部之间形成的接合空间中通过将硬化填充剂注入PCa柱构件的柱头的一个表面和PCa柱/梁连接部分块的下表面,并进入多个PCa柱/梁连接部分块的柱主加强件的插入孔解决方案:具有流动性的水泥砂浆被送入接合空间26,以使其从每个用于柱主加强件的插入孔16的下端流出,使其可以填充孔的内部。在插入孔中上升的硬化填充剂的顶端的最高顶端到达相应插入孔的上端之前,停止注入硬化填充剂,从而在插入孔的顶端附近留下未填充的部分。保证金。未填充的部分填充有从每个插入孔的上端注入的硬化填料。;版权所有:(C)2006,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号