首页> 外国专利> The tubed silicon crystalline it is produced with tubed silicon crystalline production manner and its production manner

The tubed silicon crystalline it is produced with tubed silicon crystalline production manner and its production manner

机译:以管式硅晶体的生产方式及其生产方式生产的管式硅晶体

摘要

Topic It offers the tubed silicon crystalline makes that it produces the tubed silicon crystalline from silicon raw materials without doing cutting work possible, produces with tubed silicon crystalline production manner and that production manner. SolutionsCoefficient of thermal expansion is smaller than silicon, coefficient of thermal expansion is larger than the molten liquid storage container and the silicon which were formed with the material whose melting point is high, the core which was formed with the material whose melting point is high is used. Nitriding silicon (Si3 N4) it applies to the inside of the aforementioned molten liquid storage container, and the outside of aforementioned core lays out aforementioned core inside the aforementioned molten liquid storage container. And, restoration the silicon molten liquid in the void which at the inside of the aforementioned molten liquid storage container and the outside of aforementioned core was formed, while maintaining the liquid Characteristic of the aforementioned silicon molten liquid, from base side of the aforementioned molten liquid storage container it provides temperature gradient to above, makes the aforementioned silicon molten liquid solidify. Choice figure Drawing 1
机译:它提供管式硅晶体使得它可以不用切割就可以从硅原料生产管式硅晶体,以管式硅晶体的生产方式和那种生产方式来生产。解决方案热膨胀系数小于硅,热膨胀系数大于熔融液体存储容器和由熔点高的材料形成的硅,由熔点高的材料形成的芯为用过的。将氮化硅(Si 3 N 4 )应用于上述熔融液存储容器的内部,并且上述芯的外部将上述芯布置在上述熔融液的内部储存容器。并且,在保持上述硅熔融液的液体特性的同时,从上述熔融液的基部侧在形成于上述熔融液收纳容器的内部和上述芯的外侧的空隙中恢复硅熔融液。贮藏容器可向上方提供温度梯度,使上述硅熔融液凝固。 <选择图>图1

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号