METHOD FOR AIRTIGHTLY JOINING REINFORCED PLATINUM HOLLOW TUBE WITH PLATINUM FLANGE

机译:白金法兰直接连接增强白金空心管的方法

摘要

The present invention provides a new method for airtightly joining a hollow tube made of a reinforced platinum and a flange made of platinum or a platinum alloy, which prevents decreasing of mechanical strength of the hollow tube made of a reinforced platinum due to its joining with a flange.;A method for airtightly joining a hollow tube made of a reinforced platinum with a flange made of platinum or a platinum alloy, which is a method for airtightly joining the outer periphery of a hollow tube made of a reinforced platinum produced by dispersing metal oxides in platinum or a platinum alloy, with a flange made of platinum or a platinum alloy, the method comprising a step of shrink-fitting a ring made of platinum or a platinum alloy to the outer periphery of the hollow tube, a step of heating the hollow tube to which the ring is shrink-fit at from 1,150 to 1,450° C. for from 1 to 10 hours, and a step of welding the flange made of platinum or a platinum alloy to the outer periphery of the ring.
机译:本发明提供了一种新方法,该新方法将由增强铂制成的中空管与由铂或铂合金制成的法兰气密地接合,从而防止了由增强铂制成的中空管与金属铂的接合而降低机械强度。一种将由增强铂制成的空心管与由铂或铂合金制成的法兰气密连接的方法,该方法是将由分散的金属制成的由增强铂制成的空心管的气密连接。铂或铂合金中的氧化物,具有由铂或铂合金制成的凸缘,该方法包括将由铂或铂合金制成的环收缩配合到中空管的外周的步骤,加热步骤将该环在1,150至1,450℃下收缩配合的中空管1至10小时,并且将由铂或铂合金制成的凸缘焊接至该管的外周。响。

著录项

  • 公开/公告号US2011005631A1

    专利类型

  • 公开/公告日2011-01-13

    原文格式PDF

  • 申请/专利权人 KAZUO HAMASHIMA;MICHITO SASAKI;

    申请/专利号US20100884702

  • 发明设计人 KAZUO HAMASHIMA;MICHITO SASAKI;

    申请日2010-09-17

  • 分类号F16L9/00;C03B7/084;

  • 国家 US

  • 入库时间 2022-08-21 18:15:50

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号