首页> 外国专利> ACRYLONITRILE COPOLYMER AND METHOD FOR PRODUCING THE SAME, ACRYLONITRILE COPOLYMER SOLUTION AND POLYACRYLONITRILE PRECURSOR FIBER FOR CARBON FIBER AND METHOD FOR PRODUCING THE SAME

ACRYLONITRILE COPOLYMER AND METHOD FOR PRODUCING THE SAME, ACRYLONITRILE COPOLYMER SOLUTION AND POLYACRYLONITRILE PRECURSOR FIBER FOR CARBON FIBER AND METHOD FOR PRODUCING THE SAME

机译:丙烯腈共聚物及其制备方法,碳纤维的丙烯腈共聚物溶液和聚丙烯腈前体纤维及其制备方法

摘要

Disclosed are an acrylonitrile copolymer excellent in thermal stability as a solution (spinning dope) when dissolved in an amide solvent and capable of forming dense polyacrylonitrile fiber suitable for production of carbon fiber, an acrylonitrile copolymer solution in which the acrylonitrile copolymer is dissolved in an amide solvent, and a method for producing polyacrylonitrile precursor fiber for carbon fiber by use of the acrylonitrile copolymer solution. Specifically, an acrylonitrile copolymer contains a sulfonate group derived from a polymerization initiator in an amount of 1.0×10−5 equivalent/g or more, and the value (equivalent ratio) of (the content of a sulfate group derived from the polymerization initiator/the total content of the sulfonate group and the sulfate group) is 0.4 or less; an acrylonitrile copolymer solution contains the aforementioned acrylonitrile copolymer and an amide solvent.
机译:公开了当溶解在酰胺溶剂中时作为溶液(纺丝原液)具有优异的热稳定性并且能够形成适合于生产碳纤维的致密聚丙烯腈纤维的丙烯腈共聚物,其中丙烯腈共聚物溶解在酰胺中的丙烯腈共聚物溶液。溶剂,以及通过使用丙烯腈共聚物溶液生产用于碳纤维的聚丙烯腈前体纤维的方法。具体地,丙烯腈共聚物包含衍生自聚合引发剂的磺酸根基团的量为1.0×10 Sup-5 -Suppeeq / g以上,并且其值(当量比)为(硫酸盐的含量)。源自聚合引发剂的基团(磺酸根基团和硫酸根基团的总含量)为0.4以下。丙烯腈共聚物溶液包含上述丙烯腈共聚物和酰胺溶剂。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号