In sulfate resistant cement obtained by mixing ground granulated blast furnace slag, Portland cement, and high-dissolution rate gypsum for raising the sulfate resistance, the high-dissolution rate gypsum differs in grain size and specific gravity from the Portland cement, so uniform mixture is not easy. To obtain sulfate resistant cement exhibiting homogeneous initial solidification, it is important to uniformly mix the blast furnace slag, Portland cement, and high-dissolution rate gypsum.;Therefore, by premixing ground granulated blast furnace slag with an alumina content of 12 to 17.5% with high-dissolution rate gypsum and then mixing in Portland cement, it is possible to obtain uniformly mixed sulfate resistant cement.;At this time, the high-dissolution rate gypsum may be hemihydrate gypsum, type III anhydrous gypsum, or anhydrous gypsum with a specific surface area of 8000Blaine or more.
机译:为了提高耐硫酸盐性,将粉碎的高炉矿渣,波特兰水泥和高溶解率石膏混合而得的耐硫酸盐水泥,由于高溶解率石膏的粒径和比重与波特兰水泥不同,因此混合均匀。不容易。为了获得具有均匀初始凝固性能的耐硫酸盐水泥,重要的是将高炉矿渣,硅酸盐水泥和高溶解率石膏均匀混合;因此,通过预混合氧化铝含量为12%至17.5%的磨碎的高炉矿渣将高溶出率的石膏与波特兰水泥混合后,就可以获得均匀混合的耐硫酸盐水泥。这时,高溶出率的石膏可以是半水合石膏,III型无水石膏或无水石膏。比表面积为8000 Blaine 或更高。

著录项

  • 公开/公告号US2011214591A1

    专利类型

  • 公开/公告日2011-09-08

    原文格式PDF

  • 申请/专利权人 TETSUHARU IBARAKI;YUKIHIKO NAGAO;

    申请/专利号US20090737892

  • 发明设计人 TETSUHARU IBARAKI;YUKIHIKO NAGAO;

    申请日2009-08-19

  • 分类号C04B7/19;C04B22/04;

  • 国家 US

  • 入库时间 2022-08-21 18:13:10

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号