METHOD OF PREVENTING CARBON FRICTION MATERIAL ANTI OXIDATION SYSTEM MIGRATION BY UTILIZING CARBON VAPOR DEPOSITION

机译:利用碳蒸气沉积防止碳摩擦材料抗氧化系统迁移的方法

摘要

Method of protecting carbon-carbon composite brake disc against migration of anti-oxidant composition through the porosity of the composite brake disc. The method starts with a porous carbon-carbon composite brake disc, and densifies it to a density of 1.70 grams per cubic centimeter or higher. The densified brake disc is then machine to the required dimensions. The pores in the densified brake disc are closed by subjecting it to CVD/CVI processing employing (i) a gaseous feedstock comprising natural gas spiked with 10 to 25% of a more reactive gas, and/or (ii) a temperature in the range of 1100° C. to 1500° C., and/or (iii) a gas pressure in the range 10 to 100 torr, and/or (iv) a gas flow rate of 300 cc/min to 450 cc/min. CVD/CVI processing carried out using these parameters deposits carbon within and closes the pores of the surface area of the carbon-carbon composite brake disc. Subsequently, an anti-oxidant solution is applied to the non-friction surfaces of the resulting carbon-carbon composite brake disc. Due to the fact that the surface pores have been closed by processing using the specified conditions, the composite brake disc resists migration of the anti-oxidant through the body of the disc to the friction surfaces thereof.
机译:保护碳-碳复合制动盘以防止抗氧化剂成分通过复合制动盘的孔隙迁移的方法。该方法从多孔碳-碳复合制动盘开始,然后将其致密化为1.70克/立方厘米或更高的密度。然后将致密的制动盘加工成所需的尺寸。致密的制动盘中的孔通过以下方法进行封闭:使用(i)包含加有10%到25%的更高反应性气体的天然气的气态原料和/或(ii)温度在1100℃至1500℃,和/或(iii)10至100托的气压,和/或(iv)300cc / min至450cc / min的气体流速。使用这些参数进行的CVD / CVI处理将碳沉积在碳-碳复合制动盘的内部并封闭其孔隙。随后,将抗氧化剂溶液施加到所得碳-碳复合制动盘的非摩擦表面上。由于通过使用指定条件进行处理已封闭了表面气孔,因此复合制动盘可阻止抗氧化剂通过盘体向其摩擦表面迁移。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号