PRODUCING METHOD OF PORCELAIN WITH THE CLOISONNE DECORATION CAPABLE OF PREVENTING THE GENERATION OF CRACKS ON A GLAZE, AND THE PORCELAIN WITH THE CLOISONNE DECORATION

机译:具有防止釉上裂纹产生的可乐松装饰的瓷器的生产方法以及可乐松装饰的瓷器

摘要

PURPOSE: A producing method of porcelain with the cloisonne decoration, and the porcelain with the cloisonne decoration are provided to perform a process of hot-melting a pendant or a spreading cloisonne powder.;CONSTITUTION: A producing method of porcelain with the cloisonne decoration comprises the following steps: molding a porcelain shape(S10); firstly firing the porcelain for 24~48hours in 1,200~1,320deg C(S20); coating a glaze on the firstly fired porcelain(S30); secondly firing the glazed porcelain for 12~36hours in 1,000~1,180deg C(S40); forming drawings on the surface of the secondly fired porcelain(S50); thirdly firing the porcelain with the drawings for 50minutes~4hours in 750~900deg C(S60); forming cloisonne pendants on the surface of the porcelain(S70); and heat processing the porcelain(S80).;COPYRIGHT KIPO 2011
机译:目的:提供一种带有景泰蓝装饰的瓷器的生产方法,并提供一种带有景泰蓝装饰的瓷器,以进行热熔垂坠或景泰蓝粉末的过程。步骤如下:成型瓷器形状(S10);首先在1200〜1320℃下烧制24〜48小时(S20);在首次烧制的瓷器上涂釉(S30);其次在1,000〜1,180℃下烧制釉瓷12〜36小时(S40);在二次烧制的瓷器表面形成图纸(S50);然后在750〜900℃下烧制带有图样的瓷器50分钟〜4小时(S60);在瓷器表面形成景泰蓝垂饰(S70);并热处理瓷器(S80)。; COPYRIGHT KIPO 2011

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号