首页> 外国专利> THERMOPLASTIC POLYESTER RESIN COMPOSITION WITH EXCELLENT MECHANICAL PROPERTIES AND THERMAL STABILITY WHILE HOLDING MOLDABILITY IN AN INJECTION PROCESS

THERMOPLASTIC POLYESTER RESIN COMPOSITION WITH EXCELLENT MECHANICAL PROPERTIES AND THERMAL STABILITY WHILE HOLDING MOLDABILITY IN AN INJECTION PROCESS

机译:注塑过程中具有出色的机械性能和热稳定性的热塑性塑料树脂组合物

摘要

PURPOSE: A thermoplastic polyester resin composition is provided to ensure excellent mechanical properties and heat resistance, and good coatability and deposition due to excellent surface property after injection molding. ;CONSTITUTION: A thermoplastic polyester resin composition includes (a) 44.5-69.7 weight% of a polybutylene terephthalate resin, (b) 10-20 weight% of a polyethylene terephthalate resin, (c) 0.1-3.0 weight% of an ethylene copolymer represented by as chemical formula 1 as an impact reinforcing agent, (d) 0.1-2.0 weight% of maleic anhydride-grafted polypropylene as a coupling agent in which maleic anhydride is represented by as chemical formula 2, (e) 0.1-0.5 weight% of branched fatty acid ester as an inner activator represented by chemical formula 3, and (f) 20-30 weight% of talc.;COPYRIGHT KIPO 2011
机译:用途:提供热塑性聚酯树脂组合物,以确保优异的机械性能和耐热性,以及由于注模后具有出色的表面性能而具有良好的可涂布性和沉积性。 ;组成:一种热塑性聚酯树脂组合物,包含:(a)44.5-69.7重量%的聚对苯二甲酸丁二酯树脂,(b)10-20重量%的聚对苯二甲酸乙二醇酯树脂,(c)0.1-3.0重量%的乙烯共聚物通过作为化学式1作为抗冲增强剂,(d)0.1-2.0重量%的马来酸酐接枝的聚丙烯作为偶联剂,其中马来酸酐由化学式2表示。(e)0.1-0.5重量%的支链脂肪酸酯作为化学式3表示的内部活化剂,以及(f)滑石粉的20-30重量%.; COPYRIGHT KIPO 2011

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号