METHOD OF MANUFACTURING OF CARBON FIBERS REINFORCED COMPOSITES IMPROVED MECHANICAL INTERFACE STRENGTH

机译:碳纤维增强复合材料的制造方法提高了机械界面强度

摘要

PURPOSE: A carbon fiber strengthening complex production method with improved mechanical interfacial strength is provided to improve a mechanical interfacial strength with a thermoplastic matrix by using a carbon fiber sizing processed with a sizing agent as a reinforcing agent. CONSTITUTION: The carbon fiber strengthening complex production method is processed by dipping the carbon fiber into a sizing agent. A sizing bath exposure time of the carbon fiber is 10 second to 60 minutes and the carbon fiber is included within a finally manufactured composite to 10-50 weight%. In the carbon fiber strengthening composite production, a suitable temperature for heating press is 200- 265C and its suitable pressure is 2.0 to 10.0 MPa.
机译:目的:提供一种具有改善的机械界面强度的碳纤维增强复合物生产方法,以通过使用经上浆剂作为增强剂处理的碳纤维上浆剂来改善与热塑性基质的机械界面强度。组成:碳纤维增强复合材料的生产方法是将碳纤维浸入上浆剂中进行加工。碳纤维的上浆浴暴露时间为10秒至60分钟,并且碳纤维以10-50重量%的量包含在最终制造的复合物中。在碳纤维增强复合材料生产中,加热压机的合适温度为200-265℃,合适的压力为2.0至10.0 MPa。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号