首页> 外国专利> Process for preparing copper nanowire and copper nanowire prepared by the same

Process for preparing copper nanowire and copper nanowire prepared by the same

机译:制备铜纳米线的方法和由其制备的铜纳米线

摘要

The present invention relates to a method for producing copper nanowires and copper nanowires produced thereby. Copper nanowires according to the present invention are prepared by adding an amine ligand, a reducing agent, a surfactant, and a nonpolar organic solvent to CuCl 2 aqueous solution, and then mixing the reaction solution to a high pressure reactor and reacting at 80 to 200 ° C. for 24 hours. The copper nanowires according to the present invention can be prepared in a very inexpensive and simple manner by reacting in an aqueous solution, which is economical and very suitable for mass production.
机译:铜纳米线的制造方法及铜纳米线技术领域本发明涉及铜纳米线的制造方法及由此制造的铜纳米线。通过将胺配体,还原剂,表面活性剂和非极性有机溶剂添加到CuCl 2 水溶液中,然后将反应溶液混合至高压,来制备根据本发明的铜纳米线。反应器并在80至200℃下反应24小时。通过在水溶液中反应,可以以非常廉价和简单的方式制备根据本发明的铜纳米线,这是经济的并且非常适合大量生产。

著录项

  • 公开/公告号KR101073808B1

    专利类型

  • 公开/公告日2011-10-13

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20080138354

  • 发明设计人 허영덕;

    申请日2008-12-31

  • 分类号B82B3;C01G3;B82Y40;

  • 国家 KR

  • 入库时间 2022-08-21 17:49:41

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号