首页> 外国专利> METHOD FOR HEAT TREATMENT OF CELLULAR STRUCTURES block catalysts iron oxide based

METHOD FOR HEAT TREATMENT OF CELLULAR STRUCTURES block catalysts iron oxide based

机译:细胞结构的热处理方法块状催化剂氧化铁基

摘要

FIELD: chemistry.;SUBSTANCE: described is a method for thermal treatment of an iron oxide-based block catalyst with a cellular structure, characterised by that thermal treatment of the blocks is carried out in steps, and specifically as follows: blocks are first dried at temperature 20-25°C for not less than 120 h and the air-dried blocks then undergo preliminary step-by-step calcination: while raising temperature to 100-110°C at a rate of 5-7°C/h, holding the blocks at temperature 100-110°C for not less than 10 h; while raising temperature to 250-270°C at a rate of 30-35°C/h, holding the blocks at temperature 250-270°C for not less than 6 h; while raising temperature to 400-410°C at a rate of 50-55°C/h, holding the blocks at temperature 400-410°C for not less than 6 h; and then raising temperature to 950-970°C at a rate of 50-60°C/h and holding the blocks at temperature 950-970°C for not less than 10 h.;EFFECT: thermal treatment method enables to obtain strong block catalysts which are resistant to thermal cycles.;3 ex
机译:技术领域:化学物质:描述了一种具有多孔结构的基于氧化铁的嵌段催化剂的热处理方法,其特征在于,所述嵌段的热处理是分步进行的,具体地如下:首先干燥嵌段在20-25°C的温度下不少于120小时,然后将风干的块逐步进行初步煅烧:以5-7°C / h的速度将温度升至100-110°C,将试块在100-110°C的温度下保持不少于10小时;在以30-35°C / h的速度将温度升高到250-270°C的同时,将块体在250-270°C的温度下保持不少于6小时;在以50-55°C / h的速度将温度升高到400-410°C的同时,将块体在400-410°C的温度下保持不少于6小时;然后以50-60°C / h的速度将温度升至950-970°C,并将块体在950-970°C的温度下保持不少于10小时;效果:热处理方法能够获得坚固的块体耐热循环的催化剂。; 3 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号