首页> 外国专利> METHOD OF PREPARING ANTISEPTIC ADDITIVE FOR DRY CONSTRUCTION MIXTURE AND ANTISEPTIC ADDITIVE FOR DRY CONSTRUCTION MIXTURE

METHOD OF PREPARING ANTISEPTIC ADDITIVE FOR DRY CONSTRUCTION MIXTURE AND ANTISEPTIC ADDITIVE FOR DRY CONSTRUCTION MIXTURE

机译:一种用于干式建筑混合料的抗粘剂的制备方法

摘要

FIELD: chemistry.;SUBSTANCE: invention relates to methods of preparing dry construction mixtures and can be used in construction engineering. The method of preparing the antiseptic additive for a dry construction mixture involves passing direct current through electrodes immersed in water, obtaining a silver colloidal solution, feeding lime into a mixing device before mixing, batching lime into the silver colloidal solution, drying the obtained lime paste which is rich in colloidal silver, grinding the obtained dry mass, sieving the obtained ground mass, finishing mixing, packing into a prepared waterproof packaging for further application. Components are in the following ratio in wt %: lime 60%; silver colloidal solution with silver concentration of 70-75 mg/l 40%. The antiseptic additive for the dry construction mixture is dry, fine powder with specific surface area less than 5000-7000 cm2/g, rich in colloidal silver with particle size 0.005-0.015 micrometres.;EFFECT: obtaining construction antiseptic with wide range of effects for volumetric modification of concrete, mortar and dry construction mixtures with minimum consumption of raw materials, high technological effectiveness of application and transportability.;2 cl, 1 ex
机译:发明领域本发明涉及制备干建筑混合物的方法,并且可以用于建筑工程中。用于干燥建筑混合物的防腐添加剂的制备方法包括使直流电通过浸入水中的电极,获得银胶体溶液,在混合之前将石灰加入混合装置中,将石灰配料到银胶体溶液中,干燥所获得的石灰糊。将其富含胶态银,研磨得到的干燥物料,过筛得到的研磨物料,完成混合,包装成准备好的防水包装,以备后用。组分以重量%计为以下比率:石灰60%;和银胶体溶液,银浓度为70-75 mg / l 40%。用于干建筑混合物的防腐添加剂是干燥的细粉,比表面积小于5000-7000 cm 2 / g,富含胶体银,粒径为0.005-0.015微米。具有广泛作用的建筑防腐剂,可对混凝土,砂浆和干建筑混合物进行体积改性,同时减少了原材料消耗,应用和运输的技术效率高。; 2 cl,1 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号