FIELD: medicine, pharmaceutics.;SUBSTANCE: invention refers to medicine. There is described method of producing calcium-phosphate micro/nanostructure samples which includes dispersion of a hydroxyapatite target Ca10(PO)6(OH)2 in a vacuum chamber in an argon or oxygen atmosphere at a distance of the target and substrate holder 40 to 50 mm, while the micro/nanostructures are produced at high-frequency discharge power density 0.1 to 0.5 Wt/cm2, argon or oxygen pressure 0.1 to 1 Pa, negative bias 90 to 100 V with moulding time 15 to 180 minutes.;EFFECT: invention aims at extending the range of products and can be used in dentistry, traumatology and orthopaedics.;3 cl, 7 dwg, 1 tbl
机译:领域:药物,药品;物质:发明是指药物。描述了一种制备磷酸钙微/纳米结构样品的方法,该方法包括分散羟基磷灰石靶标Ca 10 (PO) 6 (OH) 2 2 < / Sup>,氩气或氧气压力0.1到1 Pa,负偏压90到100 V,成型时间15到180分钟。效果:本发明旨在扩大产品范围,可用于牙科,创伤学和骨科。 3厘升,7桶,1桶

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号