首页> 外国专利> Self-compacting concrete comprises portion of blast furnace cement, which contains portion of Portland cement clinker and portion of blast furnace slag, portion of limestone flour, and portion of coarse aggregate made of sand or gravel

Self-compacting concrete comprises portion of blast furnace cement, which contains portion of Portland cement clinker and portion of blast furnace slag, portion of limestone flour, and portion of coarse aggregate made of sand or gravel

机译:自密实混凝土包括一部分高炉水泥,一部分波特兰水泥熟料,一部分高炉矿渣,一部分石灰石粉以及一部分由沙子或砾石制成的粗骨料

摘要

The self-compacting concrete comprises a portion of 340 kg blast furnace cement per m 3concrete, where the blast furnace cement contains a portion of Portland cement clinker (20-34%) and a portion of blast furnace slag (66-80%), a portion of 300 kg limestone flour per m 3concrete, a portion of 1400 kg coarse aggregate made of sand, gravel or crushed stone per m 3concrete, where the coarse aggregate has an aggregate size of maximum 8 mm, a styrene-acrylate copolymer with a portion of 5-15% to the mass of the blast furnace cement, and a high performance solvent. The self-compacting concrete comprises a portion of 340 kg blast furnace cement per m 3concrete, where the blast furnace cement contains a portion of Portland cement clinker (20-34%) and a portion of blast furnace slag (66-80%), a portion of 300 kg limestone flour per m 3concrete, a portion of 1400 kg coarse aggregate made of sand, gravel or crushed stone per m 3concrete, where the coarse aggregate has an aggregate size of maximum 8 mm, a styrene-acrylate copolymer with a portion of 5-15% to the mass of the blast furnace cement, a high performance solvent based on polycarboxylate ether with a portion of maximum 2% to the mass of the blast furnace cement and with a water/cement ratio of maximum 0.5, and color pigments. An independent claim is included for a method for producing a self-compacting concrete.
机译:自密实混凝土每m 3>混凝土包含一部分340公斤高炉水泥,其中高炉水泥包含一部分波特兰水泥熟料(20-34%)和一部分高炉矿渣(66-80%) ),每m 3>混凝土中有300公斤石灰石粉,每m 3>混凝土中有1400公斤由沙子,砾石或碎石制成的粗骨料,其中粗骨料最大粒径为8 mm,含量为高炉水泥质量的5-15%的苯乙烯-丙烯酸酯共聚物和高性能溶剂。自密实混凝土每m 3>混凝土包含一部分340公斤高炉水泥,其中高炉水泥包含一部分波特兰水泥熟料(20-34%)和一部分高炉矿渣(66-80%) ),每m 3>混凝土中有300公斤石灰石粉,每m 3>混凝土中有1400公斤由沙子,砾石或碎石制成的粗骨料,其中粗骨料最大粒径为8 mm,含量占高炉水泥质量的5-15%的苯乙烯-丙烯酸酯共聚物,一种基于聚羧酸盐醚的高性能溶剂,其含量占高炉水泥的质量的最大2%以及水/水泥比例最大为0.5,与彩色颜料有关。本发明包括一种用于制造自密实混凝土的方法的独立权利要求。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号