PROBLEM TO BE SOLVED: To provide a material which can be used for low pressure molding, and which has a low core loss while taking advantage of the characteristic of amorphous powder that is the high coercive force.;SOLUTION: There is provided a composite magnetic material comprising: a magnetic powder material containing, based on the weight of the magnetic powder material, 45 to 80 wt.% of amorphous powder and 55 to 20 wt.% of crystalline powder; and a binder. Here, the magnetic powder material contains, based on the weight thereof, 4.605 to 6.60 mass% of Si, 2.64 to 3.80 mass% of Cr, 0.225 to 0.806 mass% of C, 0.018 to 0.432 mass% of Mn, 0.99 to 2.24 mass% of B, 0.0248 mass% or less of P, 0.0165 mass% or less of S, 0.0165 mass% or less of Co, and Fe and inevitable impurities as the remainder.;COPYRIGHT: (C)2012,JPO&INPIT
机译:解决的问题:提供一种可用于低压成型的材料,该材料具有低的铁损,同时又利用了具有高矫顽力的非晶态粉末的特性。一种材料,包括:磁性粉末材料,基于该磁性粉末材料的重量,其包含45至80重量%的非晶粉末和55至20重量%的结晶粉末;和和粘合剂。此处,磁性粉末材料基于其重量包含4.605〜6.60质量%的Si,2.64〜3.80质量%的Cr,0.225〜0.806质量%的C,0.018〜0.432质量%的Mn,0.99〜2.24质量。 B的%,P的0.0248质量%以下,S的0.0165质量%以下,Co和Fe的0.0165质量%以下,以及不可避免的杂质作为残留量;版权所有(C)2012

著录项

  • 公开/公告号JP2012160726A

    专利类型

  • 公开/公告日2012-08-23

    原文格式PDF

  • 申请/专利权人 SUMIDA CORPORATION;

    申请/专利号JP20120009046

  • 发明设计人 NAKAMURA AKIHIKO;

    申请日2012-01-19

  • 分类号H01F1/153;H01F1/20;H01F1/26;C22C45/02;C22C38;B22F1;

  • 国家 JP

  • 入库时间 2022-08-21 17:44:16

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号