PROBLEM TO BE SOLVED: To provide a method for manufacturing a porous sintered body of titanium, which can efficiently provide the porous sintered body of titanium of high quality at a low cost.;SOLUTION: This manufacturing method comprises: a slurry production step S1 which mixes an organic binder, a foaming agent, a plasticizer, water and a surface-active agent as needed, with at least one of a titanium powder and a titanium hydride powder to produce slurry; a forming step S2 which applies the slurry on a first support to form a formed article; a foaming step S3 which produces a formed and foamed article by heating, drying and foaming the formed article; a degreasing step S4 which heats and degreases the formed and foamed article that has been separated from the first support and mounted on a second support; a first sintering step S5 which produces a primary sintered body having electroconductivity by heating the degreased, formed and foamed article in a non-oxidative atmosphere; and a second sintering step S7 which produces the porous sintered body of titanium by sintering the primary sintered body in a non-oxidative atmosphere at a temperature higher than that in the first sintering step.;COPYRIGHT: (C)2009,JPO&INPIT
机译:解决的问题:提供一种制造钛的多孔烧结体的方法,该方法可以有效地以低成本提供高质量的钛的多孔烧结体;解决方案:该制造方法包括:浆料生产步骤S1,根据需要将有机粘合剂,发泡剂,增塑剂,水和表面活性剂与钛粉和氢化钛粉中的至少一种混合以制备浆料;形成步骤S2,其将浆料施加在第一载体上以形成成形品;发泡步骤S3,其通过加热,干燥和发泡成型制品来生产成型发泡制品。脱脂步骤S4,其加热和脱脂已与第一支撑件分离并安装在第二支撑件上的发泡制品。第一烧结步骤S5,其通过在非氧化性气氛中加热脱脂,成型和发泡的制品来产生具有导电性的初级烧结体;第二烧结步骤S7,其通过在比第一烧结步骤更高的温度下在非氧化气氛中烧结一次烧结体来制造钛的多孔烧结体。版权所有:(C)2009,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号