The instant pulse filter according to the present invention, which may cause a malfunction or a short life span of a semiconductor device, is made using an aluminum anodic oxidation, comprisinga first step for forming an aluminum thin film layer on an upper side of an insulator substrate; a second step for forming an aluminum oxide thin film layer having a pore by oxidizing the aluminum thin film layer by means of an anodic oxidation; a third step for depositing a metallic material on an upper side of the aluminum thin film layer for filling the pore; a fourth step for forming a nano rod in the interior of the aluminum oxide thin film layer by eliminating the metallic material deposited except in the pore; a fifth step for forming an internal electrode on an upper side of the aluminum oxide thin film layer having the nano rod; a sixth step for forming a protective film layer on an upper side of the same in order to protect the aluminum oxide thin film layer and the internal electrode from the external environment; and a seventh step for forming an external electrode on both sides of the substrate in which the protective film layer is formed.
机译:根据本发明的可能引起半导体器件的故障或寿命短的瞬时脉冲滤波器是使用铝阳极氧化制成的,包括在绝缘体的上侧形成铝薄膜层的第一步。基质;第二步骤是通过阳极氧化将铝薄膜层氧化而形成具有孔的氧化铝薄膜层的步骤。第三步骤,在铝薄膜层的上侧沉积金属材料以填充孔;第四步骤,通过除去除了孔中沉积的金属材料,在氧化铝薄膜层的内部形成纳米棒。第五步骤,在具有纳米棒的氧化铝薄膜层的上侧形成内部电极。第六步骤,在保护膜层的上侧形成保护膜层,以保护氧化铝薄膜层和内部电极不受外部环境的影响;第七步骤,用于在形成有保护膜层的基板的两面上形成外部电极。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号