PROBLEM TO BE SOLVED: To prepare a coating material for precoated steel plates using a low priced polyacrylic resin and giving better wheatherability and stain resistance, and to provide a precoated steel plate and panels for roof walls or the like using the same, and to provide a method for producing the precoated steel plate. ;SOLUTION: This coating material is prepared by including both (A) an acrylic polyol-based copolymer obtained from a polymerizable monomer for stabilization to ultraviolet light, a polymerizable monomer having a cycloalkyl group and a polymerizable monomer having a hydroxyl group as essential monomers and (B) a fluororesin powder containing polytetrafluoroethylene. The coating material is applied to at least one side of steel plate in a coating thickness of 1-25 m and is baked at the plate temperature of 150C and 320C to produce precoated steel plate excellent in weather resistance and stain resistance.;COPYRIGHT: (C)1999,JPO
机译:解决的问题:使用低价的聚丙烯酸树脂制备用于预涂钢板的涂料,并提供更好的耐小麦性和耐污性,并提供用于屋顶等的预涂钢板和面板,并提供一种制备预涂钢板的方法。 ;解决方案:该涂料的制备方法是将(A)丙烯酸多元醇类共聚物(由用于稳定紫外线的可聚合单体,具有环烷基的可聚合单体和具有羟基的可聚合单体)作为基本单体制成,并(B)含有聚四氟乙烯的氟树脂粉末。将涂层材料以1-25 m的涂层厚度涂在钢板的至少一侧上,并在150°C和<320°C的板温下烘烤,以生产出具有极好的耐候性和耐污染性的预涂层钢板。 (C)1999,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号