PPROBLEM TO BE SOLVED: To provide a high-strength concrete composition using a silica fume slurry where a concrete structure has superior strength, especially not only the outer part of the concrete structure but also a core part are satisfied with a specified design standard strength (for example, 130 N/mmSP2/SP), and to provide a method for producing the same. PSOLUTION: The high-strength concrete composition using the silica fume slurry includes low-heat portland cement, moderate-heat portland cement, the silica fume slurry, a fine aggregate, a coarse aggregate, kneading water and a high performance AE water reducing agent. The content of silica fume composing the silica fume slurry is 8-15 mass% to the total amount of the low-heat portland cement, the moderate-heat portland cement and the silica fume. The blending ratio of the low-heat portland cement and the medium-heat portland cement is 4:6-6:4 in mass ratio. PCOPYRIGHT: (C)2011,JPO&INPIT
机译:

要解决的问题:提供一种使用硅粉浆料的高强度混凝土组合物,其中混凝土结构具有优异的强度,特别是不仅混凝土结构的外部而且核心部分都满足指定的设计要求标准强度(例如130 N / mm 2 ),并提供一种制造方法。

解决方案:使用硅灰浆的高强度混凝土组合物包括低热硅酸盐水泥,中热硅酸盐水泥,硅灰浆,细骨料,粗骨料,捏合水和高性能AE水还原剂。构成硅粉浆料的硅粉的含量相对于低热硅酸盐水泥,中热硅酸盐水泥和硅粉的总量为8〜15质量%。低热硅酸盐水泥和中热硅酸盐水泥的质量比为4:6-6:4。

版权:(C)2011,日本特许厅&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号