摘要

Disclosed is a method for continuously and stably producing a CNT assembly having a high specific surface area in a catalyst activating substance-containing, high-carbon-concentration environment.;Specifically disclosed is a method for growing a carbon nanotube by contacting a feedstock gas and a catalyst-activating substance to a catalyst on a base. The method includes: a formation step of supplying and contacting a reducing gas to the catalyst on the base, and heating at least one of the catalyst and the reducing gas to reduce the catalyst and/or particulate the catalyst; and a carbon nanotube growing step of contacting a carbon-containing, oxygen-free feedstock gas and an oxygen-containing catalyst-activating substance to at least one of the catalyst and the catalyst particles, and heating at least one of the catalyst, the catalyst particles, the feedstock gas, and the catalyst-activating substance to grow the carbon nanotube, wherein the ratio of the number concentration of the carbon atoms contained in the feedstock gas used in the carbon nanotube growing step to the number concentration of the oxygen atoms contained in the catalyst-activating substance used in the carbon nanotube growing step ranges from 0.5 to 200.
机译:公开了一种在含有催化剂活性物质的高碳浓度环境下连续稳定地制造具有高比表面积的CNT组件的方法。具体而言,公开了一种通过使原料气与碳纳米管接触来生长碳纳米管的方法。将催化剂活化物质转化为碱的催化剂。该方法包括:形成步骤,将还原性气体供应和接触到基础上的催化剂,并且加热催化剂和还原性气体中的至少一种以还原催化剂和/或使催化剂颗粒化;碳纳米管生长步骤,使含碳的无氧原料气和含氧的催化剂活化物质与催化剂和催化剂颗粒中的至少一种接触,并加热催化剂,催化剂中的至少一种颗粒,原料气体和催化剂活化物质来生长碳纳米管,其中碳纳米管生长步骤中所用原料气体中所含碳原子的数量浓度与所含氧原子的数量浓度之比碳纳米管生长步骤中使用的催化剂活化物质的“ H 2 O 3”为0.5〜200。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号