embedded image ;(in the formula (1), R is a polyisocyanate residue and represents an aliphatic hydrocarbon group having 1 to 20 carbon atoms, a hydrocarbon group having an alicyclic structure and 3 to 20 carbon atoms or a hydrocarbon group having an aromatic ring and 6 to 20 carbon atoms.)"/> POLYLACTIC ACID-BASED RESIN, PROCESS FOR PRODUCING POLYLACTIC ACID-BASED RESIN, POLYLACTIC ACID RESIN COMPOSITION, STEREOCOMPLEX POLYLACTIC ACID RESIN COMPOSITION AND PROCESS FOR PRODUCING STEREOCOMPLEX POLYLACTIC ACID RESIN COMPOSITION
首页> 外国专利> POLYLACTIC ACID-BASED RESIN, PROCESS FOR PRODUCING POLYLACTIC ACID-BASED RESIN, POLYLACTIC ACID RESIN COMPOSITION, STEREOCOMPLEX POLYLACTIC ACID RESIN COMPOSITION AND PROCESS FOR PRODUCING STEREOCOMPLEX POLYLACTIC ACID RESIN COMPOSITION

POLYLACTIC ACID-BASED RESIN, PROCESS FOR PRODUCING POLYLACTIC ACID-BASED RESIN, POLYLACTIC ACID RESIN COMPOSITION, STEREOCOMPLEX POLYLACTIC ACID RESIN COMPOSITION AND PROCESS FOR PRODUCING STEREOCOMPLEX POLYLACTIC ACID RESIN COMPOSITION

机译:聚乳酸树脂,聚乳酸树脂的制造方法,聚乳酸树脂组合物,立体复合聚乳酸树脂的组成及制造立体复合聚乳酸树脂的方法

摘要

The invention provides a polylactic acid-based resin having a high molecular weight, high heat resistance and an amide bond in its molecular chain, a production process and a use thereof. The polylactic acid-based resin comprises a constituting unit represented by the following formula (1) and which is obtained by allowing a polyisocyanate compound to react with a mixture comprising at least a poly (L-lactic acid) in which the percentage of the terminal functional group which is a carboxyl group exceeds 50% and a poly (D-lactic acid) in which the percentage of the terminal functional group which is a carboxyl group exceeds 50%.; embedded image ;(in the formula (1), R is a polyisocyanate residue and represents an aliphatic hydrocarbon group having 1 to 20 carbon atoms, a hydrocarbon group having an alicyclic structure and 3 to 20 carbon atoms or a hydrocarbon group having an aromatic ring and 6 to 20 carbon atoms.)
机译:本发明提供了一种在分子链中具有高分子量,高耐热性和酰胺键的聚乳酸基树脂,其生产方法及其用途。聚乳酸类树脂包含由下式(1)表示的构成单元,并且其通过使多异氰酸酯化合物与至少包含其中末端的百分比的聚(L-乳酸)的混合物反应而获得。作为羧基的官能团超过50%,以及作为羧基的末端官能团的百分比超过50%的聚(D-乳酸)。 “嵌入式图像” (式(1)中,R为多异氰酸酯残基,表示碳原子数1〜20的脂肪族烃基,具有脂环结构且碳原子数3〜20的烃基或具有芳香环且6的烃基。到20个碳原子。)