首页> 外国专利> Process for producing polylactic acid resins, polylactic acid resins, polylactic acid resin composition, a stereocomplex polylactic acid resin composition and method of producing stereocomplex polylactic acid resin composition

Process for producing polylactic acid resins, polylactic acid resins, polylactic acid resin composition, a stereocomplex polylactic acid resin composition and method of producing stereocomplex polylactic acid resin composition

机译:制备聚乳酸树脂的方法,聚乳酸树脂,聚乳酸树脂组合物,立构复合物聚乳酸树脂组合物和制备立构复合物聚乳酸树脂组合物的方法

摘要

It possesses high heat resistance at the high-molecular quantity, the poly- lactic acid type resin which possesses amide connection in the molecular chain, it designates the production method and that its use is offered as purpose. The ratio where the terminal functional group is the carboxyl group exceeds 50%, poly- (L lactic acid) and the ratio where the terminal functional group is the carboxyl group exceeds 50%, poly- lactic acid type resin (i) the constitution unit which is obtained poly- (D lactic acid) by reacting the blend and the poriisoshianeto chemical compound which are contained at least, the below-mentioned formula is displayed with (1) is included. (Formula in (1), R being the poriisoshianeto residue, carbon count the aliphatic hydrocarbon radical of 1 - 20, the carbon count the carbon count displays the hydrocarbon radical 6 to which includes the hydrocarbon radical or aromatic ring of 3 which includes fat ring structure - 20 - 20.)
机译:它在大分子量时具有高耐热性,在分子链上具有酰胺连接的聚乳酸型树脂,指定了生产方法,并提供了其用途。聚乳酸系树脂(i)的构成单元中,末端官能团为羧基的比例超过50%,聚(L乳酸),末端官能团为羧基的比例超过50%。通过使至少含有的共混物和对苯二甲酰胺化合物反应而得到的聚(D乳酸)的下述式(1)表示。 (式(1)中,R为多异芳烃基残基,碳数为1〜20的脂肪族烃基,碳数为碳数6表示含有烃基的烃基或含有脂肪环的3为芳香环。结构-20-20。)

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号