A polylactic acid stereocomplex has a crystal melting peak temperature of 215° C. or more, wherein the crystal melting peak is a single peak and has a peak half width of 12° C. or less, and a crystal melting enthalpy of 60 J/g or more as measured by differential scanning calorimetry. The polylactic acid stereocomplex has a high melting point, good heat resistance, and a high level of mechanical properties and chemical resistance. The method for producing a polylactic acid stereocomplex includes chaotic mixing of 30 to 70 parts by weight of (A) poly-L-lactic acid and 30 to 70 parts by weight of (B) poly-D-lactic acid based on 100 parts by weight of the total of (A) poly-L-lactic acid and (B) poly-D-lactic acid.
机译:聚乳酸立体复合物的结晶熔融峰温度为215℃以上,其中结晶熔融峰为单峰,且峰的半峰宽为12℃以下,结晶熔融焓为60J /。通过差示扫描量热法测定的结果为g以上。聚乳酸立体复合物具有高熔点,良好的耐热性以及高水平的机械性能和耐化学性。聚乳酸立体复合体的制造方法,相对于100重量份的聚乳酸,将30〜70重量份的(A)聚-L-乳酸与30〜70重量份的(B)的聚D-乳酸进行混沌混合。 (A)聚-L-乳酸和(B)聚-D-乳酸的总重量。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号