摘要

A noncrystalline composite alkali metal titanate composition which is chemically stable, outstanding in resistance to hygroscopicity and suited as base materials for friction materials. The said composition comprises at least 60 wt. % of an alkali metal titanate represented by the general formula M2O.nTiO2 wherein M is one or at least two alkali metal elements and n is a number of 1 to 4, and at least 10 wt. % of SiO2, M2O/SiO2 being equal to or less than 2.5. When desired, it is possible to incorporate into the composition an oxide of at least one element selected from the group consisting of B, Mg, Al, P, Ca and Zn, and/or an oxide of at least one element selected from the group consisting of V, Cr, Mn, Fe, Co, Ni, Cu, Y, Zr, Nb and Ba.
机译:一种非晶体复合碱金属钛酸盐组合物,该组合物化学稳定,耐吸湿性优异,适合用作摩擦材料的基础材料。所述组合物包含至少60重量%。通式M 2 O.nTiO 2 表示的碱金属钛酸盐的%,其中M是一种或至少两种碱金属元素,n是1到2的数4,至少10 wt。 SiO 2 ,M 2 O / SiO 2 的百分比等于或小于2.5。如果需要,可以将选自B,Mg,Al,P,Ca和Zn的至少一种元素的氧化物和/或选自该组的至少一种元素的氧化物掺入组合物中。由V,Cr,Mn,Fe,Co,Ni,Cu,Y,Zr,Nb和Ba组成。

著录项

  • 公开/公告号US8093171B2

    专利类型

  • 公开/公告日2012-01-10

    原文格式PDF

  • 申请/专利权人 KENJI HIGASHI;MASAFUMI YASUDA;

    申请/专利号US20080677163

  • 发明设计人 MASAFUMI YASUDA;KENJI HIGASHI;

    申请日2008-09-12

  • 分类号C04B35/462;F16D69/04;

  • 国家 US

  • 入库时间 2022-08-21 17:25:43

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号