Method for leaching Gold comprising Cu Cu Sulphide ore leaching with silicate mineral with au au or cu to reduce the level of 7.9% by weightMixed solution of Ferric Chloride ions and chloride ions or to Trivalent Iron and Iron oxidized by Bubbling Air, Adjust pH to 1.9, Shake and Leach.
机译:一种含金的浸出方法,包括用金或铜与硅酸盐矿物浸提铜铜硫化物矿石以降低7.9%(重量)含量的三氯化铁离子和氯离子混合溶液或三价铁和鼓泡空气氧化的铁,将pH值调节至1.9 ,摇一摇和浸出。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号