首页> 外国专利> Process to increase the adsorption capacity of Powdered Activated Carbon and Activated Carbon without dispersion.

Process to increase the adsorption capacity of Powdered Activated Carbon and Activated Carbon without dispersion.

机译:增加粉末状活性炭和无分散活性炭吸附能力的工艺。

摘要

"Process to increase the adsorption capacity of Activated Carbon Powder and Manufacture of Activated Carbon without dispersion" Where the activated Charcoal with Steam and air at a high temperature, Acidic Solutions and washed with water to remove the mineral compounds (ASH) and Bo Lsas Air left in the Pores.In order to obtain a product with a humidity content linked from 25 to 40%, high purity, ultra-fine particles free (under 5 microns) of Coal, with easy access of adsorbates, and in the Next Stage, The Coal can be used in purification of liquid, presentand Or High Efficiency Index, with higher speed of adsorption of Organic impurities,In the form of small molecules that roughly correspond to more volatile compounds such as water, odors, Flavors and many Solvents, and large molecules such as those that are coloured or Humic substance (Humic and Fulvic acids) that is generated by DECOMPOSING The organic matter.Activated Carbon thus produced has the advantage of not producing Dust in handling or during the process of preparing the suspension and subsequent implementation in the purification process, using a smaller amount of Dry Coal base, a lower amount of auxiliary filtraciu00f3 In the stage of Coal Separation Fluid, generating less waste SolidUsing less labor, less consumption of Energy in the preparation of the suspension of Coal for its subsequent implementation, and Lower consumption of water in the washing of the filter when used in Bleaching processes of glucose syrups Sugar syrups, Glice or discolouration Rina.
机译:“增加活性炭粉的吸附能力的过程和不分散的活性炭的制造”其中活性炭用蒸汽和空气在高温,酸性溶液中并用水洗涤以除去矿物化合物(ASH)和Bo Lsas Air留在毛孔中。为了获得湿度在25%至40%之间的产品,高纯度,不含煤的超细颗粒(5微米以下),易于吸收被吸附物。阶段,煤可用于提纯液体,现有和或高效率指数,并具有较高的有机杂质吸附速度,呈小分子形式,大致对应于易挥发的化合物,例如水,气味,香精和许多溶剂以及通过分解有机物而产生的大分子,例如有色分子或腐殖质(腐殖酸和富勒酸),这样产生的活性炭的优点是不会在处理或在制备悬浮液的过程中以及随后在提纯过程中实施的过程中,使用较少量的干煤基料,较少量的助滤剂在选煤阶段,产生的废料更少,固体更少,劳动更少在准备用于后续实施的煤的悬浮液时消耗能量,以及在用于葡萄糖浆的漂白过程中,在过滤器的洗涤过程中降低水的消耗糖浆,糖浆或变色丽娜。

著录项

  • 公开/公告号CO6350192A1

    专利类型

  • 公开/公告日2011-12-20

    原文格式PDF

  • 申请/专利权人 WIEDEMANN TREJOS AYMER;

    申请/专利号CO20110118122

  • 发明设计人 WIEDEMANN TREJOS AYMER;

    申请日2011-09-13

  • 分类号C01B31/00;

  • 国家 CO

  • 入库时间 2022-08-21 17:25:20

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信