首页> 外国专利> NICKEL OXIDE POWDER MATERIAL FOR SOLID OXIDE FUEL CELL, PROCESS FOR PRODUCING THE NICKEL OXIDE POWDER MATERIAL, AND FUEL ELECTRODE MATERIAL, FUEL ELECTRODE, AND SOLID OXIDE FUEL CELL USING THE NICKEL OXIDE POWDER MATERIAL

NICKEL OXIDE POWDER MATERIAL FOR SOLID OXIDE FUEL CELL, PROCESS FOR PRODUCING THE NICKEL OXIDE POWDER MATERIAL, AND FUEL ELECTRODE MATERIAL, FUEL ELECTRODE, AND SOLID OXIDE FUEL CELL USING THE NICKEL OXIDE POWDER MATERIAL

机译:用于固体氧化物燃料电池的镍氧化物粉末材料,用于生产镍氧化物粉末材料的过程以及使用镍氧化物粉末材料的燃料电极材料,燃料电极和固体氧化物燃料电池的过程

摘要

A nickel oxide powder material that can restrain cracking of electrode due to oxidation expansion and peeling from a electrolyte and thus can decrease deterioration of the power generation characteristics, even in the case that the anode is exposed to an oxidizing atmosphere caused by the disruption of the fuel supply at operating temperature or the like when used as an anode material for a solid oxide type fuel cell and its efficient production method, and the anode material for the solid oxide type fuel cell using the nickel oxide powder material, are provided. The nickel oxide powder material for an anode material constituting a solid oxide type fuel cell is characterized in that it is made up of a core particle (a) composed of a nickel oxide fine particle and a coating layer (b) including a zirconium hydroxide, which is formed on the surface of the core particle (a), as its main component, and that the zirconium content contained in the coating layer (b) is 0.001 to 0.01 g/m 2 per surface area of the nickel oxide fine particle.
机译:镍氧化物粉末材料,即使在阳极暴露于由氧化氢的破坏引起的氧化气氛中的情况下,也可以抑制由于氧化膨胀和从电解质中剥离引起的电极开裂,从而可以减少发电特性的恶化。提供了在用作固体氧化物型燃料电池的负极材料时在工作温度等下的燃料供给及其有效的制造方法,以及使用了氧化镍粉末材料的固体氧化物型燃料电池的负极材料。构成固体氧化物型燃料电池的负极材料用氧化镍粉末材料的特征在于,其由由氧化镍微粒构成的芯颗粒(a)和包含氢氧化锆的涂层(b)构成,在芯粒子(a)的表面上形成的作为主要成分的氧化锌,被覆层(b)中所含的锆含量为氧化镍微粒的每表面积0.001至0.01g / m 2。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号