The invention relates to an autocompressing asphalt mixture, in particular a mastic asphalt mixture, in particular for pavement coating layers, asphalt intermediate layers, asphalt binder layers, and/or asphalt compression layers, preferably of the class 0/8 or 0/5, made of chippings, sand, filler, and binding agents, as well as optionally additives, the total mass of all components being 100% by mass. Said particular mastic asphalt mixture is characterized in that the chippings content having aggregate size 1 mm is between 60% by mass and 80% by mass, that the sand content of natural and crushed sand having a grain size 0.063 mm and ≤ 2 mm is between 2% by mass and 15% by mass, that the filler content having an aggregate size ≤ 0.063 is between 12% by mass and 25% by mass, and that the binding agent content is between 6.0% by mass and 8.5% by mass.