PURPOSE: A middle-temperature asphalt pavement composition is provided to improve mid temperature construction techniques, thereby commercializing in wide range of energy-savings and low carbon technologies. CONSTITUTION: A middle-temperature asphalt pavement composition comprises 91-94 weight% of asphalt, 3-5 weight% of thermoplastic elastomer, 2-4 weight% of maleic anhydride-grafted polyethylene wax which has 4-10% of grafting ratio, and 0.1-1 weight% of process oil. The middle-temperature asphalt pavement composition has viscosity of less than 700 cP at 135 deg. Celsius. The thermoplastic elastomer is styrene-butadiene-styrene(SBS), styrene-butadiene copolymer rubber(SBR), natural rubber latex, or a combination thereof.
机译:目的:提供一种中温沥青路面组合物,以改善中温施工技术,从而实现广泛的节能和低碳技术的商业化。组成:一种中温沥青路面组合物,其包含91-94重量%的沥青,3-5重量%的热塑性弹性体,2-4重量%的马来酸酐接枝的聚乙烯蜡,接枝率为4-10%,以及0.1-1重量%的加工油。中温沥青路面组合物在135℃下的粘度小于700cP。摄氏温度热塑性弹性体是苯乙烯-丁二烯-苯乙烯(SBS),苯乙烯-丁二烯共聚物橡胶(SBR),天然橡胶胶乳或它们的组合。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号