PURPOSE: An oxygen selective absorbent with rapid absorbent rate and a method for manufacturing the same are provided to rapidly absorb oxygen from atmosphere.;CONSTITUTION: A method for manufacturing an oxygen selective absorbent with rapid absorbent rate includes the following: BaMg(CO_3)_2 particles or BaMg(CO_3)_2 particles with MgCO_3 or Mg(OH)_2 attached on the external sides are prepared; and the particles are fired at high temperatures. In the BaMg(CO_3)_2 particles with MgCO_3 or Mg(OH)_2 attached on the external sides, the molar ratio of the MgCO_3 or Mg(OH)_2 to BaMg(CO_3)_2 is 1 : 10. The BaMg(CO_3)_2 particles are prepared by dispersing the mixture of barium containing compounds and carbonate in distilled water and adding a magnesium carbonate precursor in the dispersed solution.;COPYRIGHT KIPO 2013;[Reference numerals] (AA) Absorbed amount/saturated absorbed amount; (BB) Time(minutes); (CC) Comparative example 1; (DD) Example 1; (EE) Example 2
机译:目的:提供一种具有快速吸收速率的氧选择性吸收剂及其制造方法,以从大气中快速吸收氧气。;组成:一种具有快速吸收速率的氧选择性吸收剂的制备方法包括:BaMg(CO_3)_2制备在外侧附着有MgCO_3或Mg(OH)_2的颗粒或BaMg(CO_3)_2颗粒。然后将颗粒在高温下烧制。在外侧附着有MgCO_3或Mg(OH)_2的BaMg(CO_3)_2颗粒中,MgCO_3或Mg(OH)_2与BaMg(CO_3)_2的摩尔比为1:10。BaMg(CO_3)通过将含钡的化合物和碳酸盐的混合物分散在蒸馏水中并在分散的溶液中添加碳酸镁前体来制备_2颗粒。; COPYRIGHT KIPO 2013; [参考数字](AA)吸收量/饱和吸收量; (BB)时间(分钟); (CC)比较例1; (DD)示例1; (EE)示例2

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号