PURPOSE: A thermoplastic polyurethane resin is provided to have excellent thermal resistance and cold resistance, to have low glass transition temperature, and has high mechanical strength.;CONSTITUTION: A thermoplastic polyurethane resin comprises polyol, polyisocyanate, and benzothiazole based chain extender. A manufacturing method of the thermoplastic polyurethane resin comprises a step of mixing polyol and polyisocyanate under nitrogen atmosphere, and synthesizing a prepolymer by reacting the mixture for 1-5 hours; and a step of adding thebenzthiazol based chain extender into the prepolymer, and reacting the mixture at 80-95 °C for 12-48 hours.;COPYRIGHT KIPO 2013
机译:目的:提供一种热塑性聚氨酯树脂,具有优异的耐热性和耐寒性,具有较低的玻璃化转变温度,并具有较高的机械强度。组成:一种热塑性聚氨酯树脂,包括多元醇,聚异氰酸酯和苯并噻唑基扩链剂。热塑性聚氨酯树脂的制造方法包括以下步骤:在氮气氛下将多元醇和多异氰酸酯混合,并使该混合物反应1-5小时,从而合成预聚物。将苯并噻唑类扩链剂加入到预聚物中,并使混合物在80-95℃下反应12-48小时。COPYRIGHTKIPO 2013

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号