PURPOSE: A method for manufacturing a steel product having different strengths through laser quenching and quenched steel used for the same are provided to easily reinforce a portion of a material without a pre-process.;CONSTITUTION: A method for manufacturing a steel product having different strengths through laser quenching is as follows. A material, which comprises C of 0.1~0.5%, Si of 0.1~0.5%, Mn of 0.5~3.0%, P of 0.1%, S of 0.05% or less (except 0), Cr of 0.01~1.0%, Al of 0.1% or less (except 0), Ti of 0.2% or less (except 0), B of 0.0005~0.08%, and Fe and inevitable impurities of the remaining amount, is prepared. Selected one among an Al plating layer, an Al-Si plating layer, a Zn-Ni plating layer, a Zn plating layer, a Zn-Al plating layer, and a high-temperature oxidation resistant resin layer is formed on the surface of the material. The material is molded into a molded product(201) of a desired shape. The portion of the molded product, which requires high strength, is reinforced through laser quenching.;COPYRIGHT KIPO 2012
机译:目的:提供一种通过激光淬火制造具有不同强度的钢材的方法,并且提供了一种用于该钢材的淬火钢,以在不进行预处理的情况下容易地增强材料的一部分。构成:一种制造具有不同强度的钢材的方法通过激光淬火的强度如下。一种材料,其包括0.1〜0.5%的C,0.1〜0.5%的Si,Mn〜0.5〜3.0%,P为0.1%,S为0.05%以下(0除外),Cr为0.01〜1.0%,Al。制备0.1%以下(0除外)的Ti,0.2%以下(0除外)的Ti,0.0005〜0.08%的B,以及Fe和不可避免的残留量的杂质。在铝镀层的表面上形成铝镀层,铝硅镀层,锌镍镀层,锌镀层,锌铝镀层和耐高温氧化树脂层中的一种。材料。该材料被模制成期望形状的模制品(201)。通过激光淬火加固模压产品中需要高强度的部分。; COPYRIGHT KIPO 2012

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号