High belite-containing sulphoaluminous clinker, method for the production and the use thereof for preparing hydraulic binders

机译:高含贝利特硫铝质熟料,其生产方法及其在制备水硬性粘结剂中的用途

摘要

A sulphoaluminate clinker includes as a phasic formulation, compared with the total weight of clinker: 5 to 25% of a calcium aluminoferrite phase with a formulation corresponding to the general formula C2AXF(1X), with X comprised between 0.2 and 0.8; 15 to 35% of a calcium sulphoaluminate phase yee' limit (C4A3$); 40 to 75% belite (C2S); from 0.01 to 10% of one or several minor phases selected from the group consisting of calcium sulphates, alkali sulphates, perovskite, calcium aluminates, gehlenite, free lime and periclase, and/or a vitreous phase, and additives including at least sodium and boron present in the following quantities, by weight as compared to the total weight of the clinker: from 0.1 to 5% of sodium expressed as sodium oxide and from 0.2 to 3% of boron, expressed as boron oxide, the total content of said additives being less than or equal to 15%.
机译:与熟料的总重量相比,硫铝酸盐熟料包括作为分相配方:5-25%的钙铝铁氧体相,配方对应于通式C2AXF(1X),X介于0.2和0.8之间;硫铝酸钙相的限量(C4A3 $)的15%至35%; 40至75%的贝利特(C2S);选自硫酸钙,碱式硫酸盐,钙钛矿,铝酸钙,钠钙石,游离石灰和钙镁石和/或玻璃状相的0.01至10%的一种或几种次要相,和/或至少包括钠和硼的添加剂相对于熟料的总重量,其含量按以下重量计:以氧化钠表示的钠含量为0.1%至5%,以氧化硼表示的硼含量为0.2%至3%,所述添加剂的总含量为小于或等于15%。

著录项

  • 公开/公告号KR101164901B1

    专利类型

  • 公开/公告日2012-07-23

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20077003969

  • 发明设计人 가트너 엘리스;리 관슈;

    申请日2005-07-19

  • 分类号C04B7/32;C04B28/06;

  • 国家 KR

  • 入库时间 2022-08-21 17:07:47