首页> 外国专利> METHOD AND DEVICE FOR THE PRODUCTION OF A THERMOPLASTIC CORRUGATED PIPE WITH DOUBLE WALLS WITH A CONNECTING COUPLING

METHOD AND DEVICE FOR THE PRODUCTION OF A THERMOPLASTIC CORRUGATED PIPE WITH DOUBLE WALLS WITH A CONNECTING COUPLING

机译:具有连接的双壁热塑波纹管的生产方法和装置

摘要

1. Method for the production of a continuous double-walled pipe, preferably made of thermoplastic material and having sections with a corrugated pipe and a section with a coupler, by extrusion of an external pipe (Sa) forming an external pipe in a double-walled pipe and an internal pipe (Si) forming an inner pipe in a double-walled pipe, in a molding passage (10) having at least one section with a corrugated molding surface, and at least one section with preferably smooth, cylindrical or several lko conical sleeve molding surface! wherein ! to form the corrugated portion, the outer tube (Sa) is extruded into the corrugated molding surface and brought into contact with the corrugated molding surface, while the inner tube (Si) is extruded into the outer tube (Sa) and brought into contact with the outer tube (Sa) located in contact with the corrugated molding surface in the region of the corrugation base of the outer pipe (Sa); ! to form the coupling section, the outer pipe (Sa) is extruded into the coupling molding surface and brought into contact with the coupling molding surface, while the inner pipe (Si) is extruded into the outer pipe (Sa), which is already in contact along the entire axial length with the coupling molding surface , and is brought into contact with the inner side of the outer pipe (Sa) already in contact with the clutch molding surface along the entire axial length of the clutch molding surface, during the process! different! the fact that the pressure (pa1) acting on the inner side of the outer pipe (Sa) is reduced (pa2) just before, or at the time when outside
机译:1.一种生产连续双壁管的方法,该连续双壁管优选地由热塑性材料制成,并且具有通过在双管中挤压形成外管的外管(Sa)而具有具有波纹管的部分和具有联接器的部分的方法。壁通道和在双通道壁通道中形成内管的内管(Si),在模制通道(10)中,该通道至少具有一个带波纹状模制表面的部分,至少一个部分具有光滑,圆柱形或多个lko锥形套筒成型面!其中!为了形成波纹部分,将外管(Sa)挤出到波纹成型表面中并与波纹成型表面接触,而将内管(Si)挤出到外管(Sa)中并且与波纹接触。外管(Sa)在外管(Sa)的波纹底部的区域中与波纹成型表面接触。 !为了形成联接部分,将外管(Sa)挤压到联接模制表面并使其与联接模制表面接触,同时将内管(Si)挤压到已经在内部的外管(Sa)中。在该过程中,沿整个轴向长度与联轴器成型表面接触,并与已经沿离合器成型表面的整个轴向长度与离合器成型表面接触的外管(Sa)的内侧接触。 !不同!实际上,在外部管道(Sa)的外侧之前(或外部)的压力(pa1)减小(pa2)

著录项

  • 公开/公告号RU2010120667A

    专利类型

  • 公开/公告日2011-11-27

    原文格式PDF

  • 申请/专利权人 УНИКОР ГМБХ (DE);

    申请/专利号RU20100120667

  • 发明设计人 КОССНЕР ХУБЕРТ (DE);

    申请日2008-10-18

  • 分类号B29C49;

  • 国家 RU

  • 入库时间 2022-08-21 17:06:59

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号