首页> 外国专利> ZEOLITE-CONTAINING CATALYST, METHOD OF PRODUCING SAID CATALYST AND METHOD OF CONVERTING STRAIGHT-RUN GASOLINE FRACTION TO HIGH-OCTANE GASOLINE COMPONENT WITH LOW BENZENE CONTENT

ZEOLITE-CONTAINING CATALYST, METHOD OF PRODUCING SAID CATALYST AND METHOD OF CONVERTING STRAIGHT-RUN GASOLINE FRACTION TO HIGH-OCTANE GASOLINE COMPONENT WITH LOW BENZENE CONTENT

机译:含沸石的催化剂,制备所述催化剂的方法以及将直馏汽油馏分转化为低苯含量的高辛烷值汽油成分的方法

摘要

FIELD: chemistry.;SUBSTANCE: invention relates to zeolite-containing catalysts. Described is a zeolite-containing catalyst for converting a straight-run gasoline fraction to a high-octane gasoline component with low benzene content, which contains high-silica zeolite with H-ZSM-5 type high-silica zeolite structure with silica modulus SiO2/Al2O3=30-50, in amount of 97.0-99.0 wt % and a modifying component which is at least one metal from the group: copper, tungsten, molybdenum, which is introduced into the high-silica zeolite in form of nanopowder of said metals in amount of 1.0-3.0 wt %; the catalyst is formed during thermal treatment. Described is a method of producing said catalyst, characterised by that the H-ZSM-5 type high-silica zeolite with silica modulus SiO2/Al2O3=30-50 is obtained via hydrothermal crystallisation of the reaction mixture at 120-180°C for 1-6 days, which contains sources of silicon oxide, aluminium oxide, alkali metal oxide, hexamethylene diamine and water, with further mixing of a high-silica zeolite with metal nanopowder obtained by electric blasting the wire of the metal in a medium of argon, followed by mechanochemical treatment, moulding the catalyst mass, drying and calcination. Described is a method of converting a straight-run gasoline fraction to a high-octane gasoline component with low content of benzene in the presence of the catalyst described above, wherein the conversion process is carried out at 350-425°C, volume rate of 1.0-2.0 h-1 and pressure 0.1-1.0 MPa.;EFFECT: high activity and selectivity of the catalyst.;4 cl, 1 tbl, 6 ex
机译:含沸石的催化剂技术领域本发明涉及含沸石的催化剂。描述了一种用于将直馏汽油馏分转化为苯含量低的高辛烷值汽油组分的含沸石催化剂,其包含具有H-ZSM-5型高二氧化硅沸石结构的高二氧化硅沸石,其二氧化硅模量为SiO < Sub> 2 / Al 2 O 3 = 30-50,含量为97.0-99.0 wt%,且改性组分为至少一种来自族:铜,钨,钼,其以1.0-3.0重量%的所述金属的纳米粉的形式引入到高硅沸石中;催化剂在热处理过程中形成。描述了一种制备所述催化剂的方法,其特征在于二氧化硅模量为SiO 2 / Al 2 O 3的H-ZSM-5型高硅沸石 = 30-50是通过将反应混合物在120-180°C下水热结晶1-6天而获得的,该混合物含有氧化硅,氧化铝,碱金属氧化物,六亚甲基二胺和水,以及将高硅沸石与金属纳米粉混合,该金属纳米粉是通过在氩气介质中对金属丝进行电喷砂而获得的,然后进行机械化学处理,成型催化剂物料,干燥并煅烧。描述了在上述催化剂的存在下将直馏汽油馏分转化为苯含量低的高辛烷值汽油组分的方法,其中转化过程在350-425℃,体积比1.0-2.0 h -1 和压力0.1-1.0 MPa .;作用:催化剂的高活性和选择性。; 4 cl,1 tbl,6 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号