首页> 外国专利> Fire-resistant hard polyurethane form null poly all which is obtained by the production manner, and the said production manner of the fire-resistant hard polyurethane form which uses the constituent and the said constituent for fire-resistant hard polyurethane

Fire-resistant hard polyurethane form null poly all which is obtained by the production manner, and the said production manner of the fire-resistant hard polyurethane form which uses the constituent and the said constituent for fire-resistant hard polyurethane

机译:耐火硬质聚氨酯的制造方法和使用该构成成分的耐火硬质聚氨酯形式的上述制造方式以及将上述成分用于耐火硬质聚氨酯的上述全部制造方法,均得到了耐火硬质聚氨酯形态。

摘要

PPROBLEM TO BE SOLVED: To provide a composition for manufacturing a flame-retardant hard polyurethane foam that solves such a problem that adhesive properties and flame retardancy of the foam are deteriorated when water is used as a sole expanding agent, a manufacturing method of the flame-retardant hard polyurethane foam using the composition, and the flame-retardant hard polyurethane foam obtained by the manufacturing method. PSOLUTION: The composition comprising a polyol (A), a catalyst (B), an expanding agent (C), a foam stabilizer (D) and a flame-retardant (E) is used as the composition for manufacturing the flame-retardant hard polyurethane foam, wherein (1) the polyol (A) is a composition comprising a glycerin-based polyol having a number-average molecular weight of 400-2,000 and a phthalic acid-based polyester polyol and the total amount of them is at least 50 wt.% based on the whole polyol; (2) the catalyst (B) is a composition comprising a quaternary ammonium salt catalyst (provided that the salt contains no hydroxyalkyl group) and a tertiary amine catalyst; and (3) the expanding agent (C) is water and the used amount thereof is at least 4 pts.wt. based on 100 pts.wt. of the polyol (A). PCOPYRIGHT: (C)2010,JPO&INPIT
机译:

要解决的问题:提供用于制造阻燃硬质聚氨酯泡沫的组合物,该组合物解决了当将水用作单一膨胀剂时泡沫的粘合性和阻燃性劣化的问题。使用该组合物的阻燃硬质聚氨酯泡沫,以及通过该制造方法得到的阻燃硬质聚氨酯泡沫。

溶液:包含多元醇(A),催化剂(B),膨胀剂(C),泡沫稳定剂(D)和阻燃剂(E)的组合物用作制造火焰的组合物。 -硬质聚氨酯泡沫塑料,其中(1)多元醇(A)是包含数均分子量为400-2,000的甘油基多元醇和邻苯二甲酸基聚酯多元醇的组合物,且它们的总量为至少50重量%,基于全部多元醇; (2)催化剂(B)是包含季铵盐催化剂(假设该盐不包含羟烷基)和叔胺催化剂的组合物。 (3)膨胀剂(C)是水,其使用量为至少4pts.wt。基于100pts.wt。多元醇(A)。

版权:(C)2010,日本特许厅&INPIT

著录项

  • 公开/公告号JP5206303B2

    专利类型

  • 公开/公告日2013-06-12

    原文格式PDF

  • 申请/专利权人 東ソー株式会社;

    申请/专利号JP20080265253

  • 发明设计人 玉野 豊;桑田 賢治;

    申请日2008-10-14

  • 分类号C08G18;C08G18/40;C08G18/18;C08G18/30;C08G101;

  • 国家 JP

  • 入库时间 2022-08-21 17:00:39