PREPARATION METHOD FOR LOW SHRINKAGE AE CONCRETE AND LOW SHRINKAGE AE CONCRETE

机译:低收缩率AE混凝土及低收缩率AE混凝土的制备方法

摘要

PROBLEM TO BE SOLVED: To provide a preparation method for low shrinkage AE concrete which has such multi-functions simultaneously that the entrained air of concrete after kneading is not defoamed, the air content is held stably with time and the dry shrinkage rate of the obtained hardening body is small, the occurrence of cracks is controlled, further the freezing and thawing resistance of the hardening body is excellent, and still further the void occurrence on the surface of concrete of the obtained hardened body after curing and the surface appearance is beautiful, and to provide the low shrinkage AE concrete obtained by the preparation method.;SOLUTION: The preparation method for the low shrinkage AE concrete comprises a step of adding 0.1-8.0 pts.mass of a low shrinkage reduction fluidizing agent per 100 pts.mass of cement in the base concrete to stiff-consistency base concrete that has been kneaded and mixed in advance.;COPYRIGHT: (C)2013,JPO&INPIT
机译:解决的问题:提供一种低收缩AE混凝土的制备方法,该方法具有多种功能,同时不使混炼后的夹带空气消泡,空气含量随时间稳定保持,所得干缩率高。固化体小,控制裂纹的发生,并且固化体的耐冻融性优异,并且固化后所得的固化体在混凝土表面的空洞进一步发生,并且表面美观。解决方案:低收缩AE混凝土的制备方法包括以下步骤:每100 pts质量添加0.1-8.0 pts质量的低收缩率减少流化剂。基础混凝土中的水泥到已预先捏合和混合的刚度一致的基础混凝土。;版权所有:(C)2013,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号