首页> 外国专利> Binderless zeolite adsorbent, method for producing binderless zeolite adsorbent, and method for adsorption separation of para-xylene from mixed xylene using binderless zeolite adsorbent

Binderless zeolite adsorbent, method for producing binderless zeolite adsorbent, and method for adsorption separation of para-xylene from mixed xylene using binderless zeolite adsorbent

机译:无粘结剂沸石吸附剂,无粘结剂沸石吸附剂的制造方法以及使用无粘结剂沸石吸附剂从混合二甲苯中吸附分离对二甲苯的方法

摘要

Binderless BaKX zeolitic adsorbents, methods for their production, and processes for their use in a liquid phase adsorptive separation process are provided. An adsorbent includes a binder-converted zeolite portion formed from x wt % kaolin clay binder and (100-x) wt % unconverted Zeolite X with a silica:alumina molar ratio of about 2.5. The kaolin clay binder is in the range of about 10 to about 20 wt %. Ba and K occupy cationic exchangeable sites within the adsorbent. K is in the range of about 0.25 to about 0.9% by weight and Ba is greater than about 31.6% by weight of the binderless BaKX zeolitic adsorbent. Cornstarch may be added to the Zeolite X and kaolin clay binder to increase adsorbent macro-porosity and pore volume. Productivity of the adsorbent is improved decreasing process operating costs. The mechanical strength of the adsorbent is also improved.
机译:提供了无粘合剂的BaKX沸石吸附剂,其生产方法以及它们在液相吸附分离过程中的使用方法。吸附剂包括由x重量%的高岭土粘合剂和(100-x)重量%的未转化的沸石X形成的粘合剂转化的沸石部分,其中二氧化硅:氧化铝的摩尔比为约2.5。高岭土粘合剂的含量为约10至约20重量%。 Ba和K在吸附剂内占据阳离子可交换位置。 K为无粘合剂的BaKX沸石吸附剂的约0.25重量%至约0.9重量%,并且Ba大于约31.6重量%。可以将玉米淀粉添加到沸石X和高岭土粘土粘合剂中以增加吸附剂的大孔隙率和孔体积。提高了吸附剂的生产率,降低了工艺运行成本。吸附剂的机械强度也得到改善。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号