The reforming plant of the excavated soil which includes the non- good quality remaining earth

机译:包括劣质残土在内的开挖土壤的改良设备

摘要

P To solve the shortage of dumping site for waste soil and environmental problems associated with a prior art method of disposing of soil excavated in a road construction site whereby the excavated soil is dumped into a site designated for waste soil disposal, and to alleviate the seriously worsening problems of destroying the natural environment and of diminishing natural resources necessary for road construction caused by mining road-construction materials and by converting and recycling excavated soil (surplus soil of construction works) and construction waste such as concrete lumps and asphalt lumps into a material useful for roadbed construction or pipe protection. PSOLUTION: Disclosed is a method of preparing a material useful for roadbed construction or pipe protection comprising the process of admixing excavated soil with construction waste such as concrete lumps, asphalt lumps, or a mixture thereof, the process of crushing the resulting mixture, the process of adding lime into the crushed mixture and classifying the above mixture using a sifter into groups of crushed particles namely a group of particles having a particle size of 40 to 30 mm, a group of particles having a particle size of 30 to 20 mm, a group of particles having a particle size of 20 to 7 mm, and a group of particles having a particle size of not greater than 7 mm, and the process of mixing the four groups of the crushed particles with each other at a prescribed ratio. PCOPYRIGHT: (C)2009 and JPO& INPIT
机译:

为了解决废土倾倒场的短缺和与在道路施工现场处理挖出的土壤的现有技术处理方法相关的环境问题,从而将挖出的土壤倾倒到指定用于弃土的处理位置,并减轻开采道路施工材料以及将挖掘出的土壤(建筑工程的剩余土壤)和建筑废料(例如混凝土块和沥青块)转化为废料造成的破坏自然环境和减少道路建设所需的自然资源等严重恶化的问题一种用于路基施工或管道保护的材料。

解决方案:公开了一种用于路基建筑或管道保护的材料的制备方法,该方法包括将挖掘的土壤与建筑废料(例如混凝土块,沥青块或其混合物)混合的过程,将所得混合物压碎的过程。将石灰添加到粉碎混合物中并使用筛分机将上述混合物分类为粉碎颗粒组的过程,即一组粒径为40到30毫米的颗粒,一组粒径为30到20的颗粒毫米,一组粒径为20至7毫米的颗粒和一组粒径不大于7毫米的颗粒,以及按规定将四组压碎颗粒相互混合的过程比。

版权:(C)2009和JPO&INPIT

著录项

  • 公开/公告号JP5317434B2

    专利类型

  • 公开/公告日2013-10-16

    原文格式PDF

  • 申请/专利权人 株式会社 山辰鉱産;

    申请/专利号JP20070156382

  • 发明设计人 山下辰己;

    申请日2007-06-13

  • 分类号B09B3/00;E01C3/00;C09K17/06;B09C1/02;B09C1/08;C09K103/00;

  • 国家 JP

  • 入库时间 2022-08-21 16:58:51

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号